Nylon
Brand/Filament | Settings | Comment |
---|---|---|
rigid.ink Nylon 12 | Extruder: 240C
Bed: 90-100C |
Achieved good results at 90-100C bed temperature. At 105C, print warped the EZ-Stik. |
taulman3D Nylon 910 | Extruder: 240C
Bed: 50C |
Brand/Filament | Settings | Comment |
---|---|---|
rigid.ink Nylon 12 | Extruder: 240C
Bed: 90-100C |
Achieved good results at 90-100C bed temperature. At 105C, print warped the EZ-Stik. |
taulman3D Nylon 910 | Extruder: 240C
Bed: 50C |